Mechanical Properties Metric English Comments
Shear Strength 1.373 MPa
199.1 psi
Momentive Performance Materials Silmate® RTV1473 Black, One Component, Silicone Rubber
Silmate RTV1473 silicone rubber is a black, on-component, ready-to-use sealant designed for formed-in-place gasketing applications where good oil resistance is a design consideration. RTV1473 silic..