Mechanical Properties Metric English Comments
Shear Strength 0.931 MPa
135 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR III 3/8-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 0.931 MPa
135 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRH-10/OX - 1/4 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength 0.931 MPa
135 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRH-10/OX - 3/16 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength >= 0.931 MPa
>= 135 psi
Plate Shear, W Direction, min, preliminary value obtained at .500 inch thickness
Hexcel® HexWeb® HRH-327 - 3/16 - 5.0 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a..
Shear Strength 0.931 MPa
135 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 0.931 MPa

@Time 1.80e+6 sec
135 psi

@Time 500 hour
Overlap, Nylon, 50% RH, Salt Water Immersion
3M 4000 UV 5280 Marine Adhesive/Sealant Fast Cure
3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio..
Shear Strength 0.931 MPa

@Time 1.80e+6 sec
135 psi

@Time 500 hour
Overlap, Nylon, 50% RH, Salt Water Immersion
3M 4000 UV 6580 Marine Adhesive/Sealant Fast Cure
3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio..
Shear Strength 0.931 MPa

@Time 1.80e+6 sec
135 psi

@Time 500 hour
Overlap, Nylon, 50% RH, Salt Water Immersion
3M 4000 UV 6586 Marine Adhesive/Sealant Fast Cure
3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio..
Shear Strength 0.931 MPa
135 psi
Overlap, Fir, 50% RH
3M 4200 Marine Adhesive/Sealant Fast Cure
A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds to wood, gelcoat and fiberglass. It forms watertight, weather-resistant seals on joints an..