Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.590 MPa | 85.6 psi | |
Sawbones Solid Rigid Polyurethane Foam 5 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |