Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus | 186.32 MPa | 27024 psi | ASTM D638 |
Lotte Chemical Titan TITANLENE® LDI300YY Low density polyethylene resin LDI300YY is a low density polyethylene resin for injection molding and is a barefoot grade. LDI300YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 2.. |