Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lotte Chemical Titan TITANLENE® LDI300YY Low density polyethylene resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Lotte Chemical Titan Holding Sdn. Bhd. (Former Titan Chemicals)
Trade Name TITANLENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANLENE® LDI300YY Low density polyethylene resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LDI300YY is a low density polyethylene resin for injection molding and is a barefoot grade. LDI300YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 2.1 & (c) 2.2.Applications: Medium sized moldings Cosmetic containers Bottle closures Food containersAdditives: BarefootAdvantages: High stiffness Good toughness Excellent glossInformation provided by Titan Chemicals
Physical Properties Metric English Comments
Base Resin Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Base Resin Melt Index 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 9.81 MPa
1420 psi
ASTM D638
Tensile Strength, Yield 11.8 MPa
1710 psi
ASTM D638
Elongation at Break 120 %
120 %
ASTM D638
1% Secant Modulus 186.32 MPa
27024 psi
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 87.0 °C
189 °F
resin; ASTM D1525
Brittleness Temperature -35.0 °C
-31.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 160 - 240 °C
320 - 464 °F
Mold Temperature 15.0 - 50.0 °C
59.0 - 122 °F