Dart Drop 9.20 g/micron
234 g/mil
Dow DOWLEX™ 2056A Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2056A Polyethylene is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer with improved thermal stability and is an outstanding choice for cr..
Dart Drop 9.20 g/micron
234 g/mil
ASTM-D1709
Braskem LL6801N LLDPE Blown Film Extrusion Polyethylene Copolymer
The LL6801N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains processing ..