Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 3.44 g/micron | 87.5 g/mil | ASTM D1709 |
ExxonMobil LL 1002.32 Cast Film Resin
(discontinued **) LL 1002.32 is a butene LLDPE resin designed for the cast film process. Films made from LL 1002.32 have very good tensile and toughness properties.Information provided by ExxonMobil Chemical |