Polymer Property : Dart Drop = 80.3 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 3.16 g/micron
80.3 g/mil
Calculated from thickness
SIDPEC EGYPTENE® LL 0220 AA LLDPE Film
Applications:Light and medium duty filmStretch filmFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o..