Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 3.16 g/micron | 80.3 g/mil | Calculated from thickness |
SIDPEC EGYPTENE® LL 0220 AA LLDPE Film Applications:Light and medium duty filmStretch filmFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o.. |