Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 2.20 - 8.54 g/micron | 56.0 - 217 g/mil | Average value: 5.23 g/micron Grade Count:55 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m.. |