Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 2.20 g/micron | 56.0 g/mil | F50; ASTM D1709 |
ExxonMobil Escorene® LD-104 LDPE Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer packaging film resin with excellent clarity and good stiffness. It is excellent either blown film or chill roll casting equipment. I.. |
|||
Dart Drop | 2.20 g/micron | 56.0 g/mil | F50; ASTM D1709 |
ExxonMobil Escorene® LD-708 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 15.5% vinyl acetate copolymer film resin. Film made from LD-708 exhibits good impact strength and superior heat sealability.Applications: Primal .. |
|||
Dart Drop | 2.20 g/micron | 56.0 g/mil | 1.5" Dart, 26" Drop Height; ASTM D1709 |
Chevron Phillips MarFlex® 7235 LLDPE Cast Film Resin Resin Type: Hexene CopolymerCharacteristics: Good OpticsGood drawdownExcellent processabilityCan use straight or in blends with LDPE or HDPEApplications: Bakery filmsOverwrapCoextrusionsInformation .. |
|||
Dart Drop | 2.20 g/micron | 56.0 g/mil | ASTM D1709 |
Chevron Phillips MarFlex® 7235B LLDPE Cast/Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymer, medium slip, cast/blown film resinCharacteristics: good optics, good drawdown, can be used straight or blended with LDPE or HDPE, can b.. |
|||
Dart Drop | 2.20 - 8.54 g/micron | 56.0 - 217 g/mil | Average value: 5.23 g/micron Grade Count:55 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m.. |