Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | <= 2.46 g/micron | <= 62.5 g/mil | ASTM D1709 |
ExxonMobil LL 3402.48 Cast Film Resin
(discontinued **) LL 3402.48 is a hexene medium density polyethylene cast film grade for applications requiring high strength and high stiffness. It can also be used in blown films. Films produced from this resin ex.. |
|||
Dart Drop | <= 2.46 g/micron | <= 62.5 g/mil | ASTM D1709 |
ExxonMobil LL 1235x70 Cast Film Resin
(discontinued **) LL 1235x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical |
|||
Dart Drop | <= 2.46 g/micron | <= 62.5 g/mil | ASTM D1709 |
ExxonMobil LL 1237x98 Cast Film Resin
(discontinued **) LL 1237x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical |
|||
Dart Drop | 2.46 g/micron | 62.5 g/mil | 26 in. dart; ASTM D-1709, A |
Bapolene® 200F Polyethylene, Film Grade Bapolene LD200F is a general purpose low density polyethylene for blown film extrusion applications. It contains medium levels of slip/antiblock additives. This product meets FDA standards for foo.. |
|||
Dart Drop | <= 2.46 g/micron | <= 62.5 g/mil | ASTM D1709 |
ExxonMobil LL 3404.48 Cast Film Resin
(discontinued **) LL 3404.48 is a hexene medium density polyethylene cast film grade for applications requiring high strength and high stiffness. It can also be used in blown films. Films produced from this resin ex.. |