Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 4.19 g/micron | 106 g/mil | ASTM D1709A |
Eastman D4032-F Polyethylene
(discontinued **) D4032-F is a low density, fractional-melt formulation which contains no slip and medium antiblock. It is designed for film applications requiring exceptional toughness, such as in heavy-duty shippi.. |