Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 3.02 g/micron | 76.7 g/mil | ASTM D1709 |
Braskem BF 2021 LDPE Cast Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Films for absorbents and diapers (with HDPE and LLDPE); general purpose. Information provi.. |