Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem BF 2021 LDPE Cast Film Extrusion Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem BF 2021 LDPE Cast Film Extrusion Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Films for absorbents and diapers (with HDPE and LLDPE); general purpose. Information provided by Braskem
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ASTM D1505
Thickness 38.0 microns
1.50 mil
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 12.0 MPa
1740 psi
ASTM D638
Film Elongation at Break, MD 287 %
287 %
ASTM D882
Film Elongation at Break, TD 995 %
995 %
ASTM D882
Elongation at Break 542 %
542 %
ASTM D638
Coefficient of Friction 0.43
0.43
ASTM D1894
Elmendorf Tear Strength, TD 4.40 g/micron
112 g/mil
ASTM D1922
Dart Drop 3.02 g/micron
76.7 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 35.0 MPa
5080 psi
ASTM D882
Film Tensile Strength at Break, TD 20.0 MPa
2900 psi
ASTM D882
Heat Seal Strength Initiation Temperature 105 °C
221 °F
Sealing Initial Temperature; Braskem® Method
Thermal Properties Metric English Comments
Vicat Softening Point 89.0 °C
192 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM D1003
Gloss 10.5 %
10.5 %
60° angle; ASTM D2457
Descriptive Properties Value Comments
Minimum Recommended Thickness 30 µm
Users viewing this material also viewed the following: