Dart Drop 11.3 g/micron
288 g/mil
F50; ASTM D1709
ExxonMobil Exceed™ 357C32 LDPE/Hexene Premium Cast Stretch Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 357C32 resin have outstanding tensile properties and..