Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 11.0 g/micron | 279 g/mil | F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Eastman 5290 LDPE High Clarity, Ultra-High Impact Film Resin, 12% EVA Copolymer
(discontinued **) Resin Type: VA Copolymer; Blown Film ResinCharacteristics: Excellent heat seal characteristics, Good optical properties, Excellent low temperature/high impact properties, Low coefficient of friction.. |
|||
Dart Drop | 11.0 g/micron | 279 g/mil | ASTM D1709 |
Lotte Chemical Titan TITANLENE® LDF265YZ Low density polyethylene LDF265YZ is a low density polyethylene resin for film extrusion. LDF265YZ has no slip and anti-block additives. LDF265YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |
|||
Dart Drop | 11.0 g/micron | 279 g/mil | ASTM D1709 |
Lotte Chemical Titan TITANZEX® HF7000 High density polyethylene HF7000 is a high density polyethylene resin for tubular film extrusion. HF7000 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1.. |
|||
Dart Drop | 11.0 g/micron | 279 g/mil | |
Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045 Polyethylene resin is a premier film resin for heavy duty applications. It complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications. The regulation sh.. |
|||
Dart Drop | 11.0 g/micron | 279 g/mil | |
Dow DOWLEX™ 2045A Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2045A Polyethylene blown film extrusion resin is a premier film resin for heavy duty applications. It is utilized where improved thermal stability over a broader range of processing conditi.. |
|||
Dart Drop | 11.0 g/micron | 279 g/mil | |
Dow DOWLEX™ 2245A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245A Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245A resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Dart Drop | 11.0 g/micron | 279 g/mil | |
Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245D Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245D resin is used where improved thermal stability over a broad range of processing conditions is nece.. |