Polymer Property : Dart Drop = 232 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 9.13 g/micron
232 g/mil
D1709
Westlake ELEVATE™ EF529 18.5% Ethylene Vinyl Acetate Copolymer
Westlake ELEVATE™ EF529 is an ethylene vinyl acetate copolymer with 18.5% VA. It contains no slip or antiblock and is designed for blown and cast films requiring excellent optics and low heat seal ..