Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 8.19 g/micron | 208 g/mil | F50; ASTM D1709 |
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a.. |
|||
Dart Drop | 8.19 g/micron | 208 g/mil | ASTM D1709 |
Huntsman Rexell® V3401 Blown Film Extrusion LLDPE