Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dart Drop = 2.56 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 2.56 g/micron
65.0 g/mil
ASTM D1709
Huntsman PE1080 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrapFDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under..
Dart Drop <= 2.56 g/micron
<= 65.0 g/mil
ASTM-D1709
Westlake EB171 MDPE Medium Density Polyethylene
Westlake EF171 is a MDPE resin suggested for use in shrink packaging applications. This material has good TD shrinkage, good optical properties, excellent machinability, and toughness. This resin gr..
Dart Drop 2.56 g/micron
65.0 g/mil
ASTM D1709
Formosa Plastics Formolene® L42022B Film (Butene Grade) LLDPE
Butene Copolymer (Barefoot)Applications: Blown and cast filmBlown and cast filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of p..
Dart Drop 2.56 g/micron
65.0 g/mil
ASTM D1709
Formosa Plastics Formolene® L42022E2 Film (Butene Grade) LLDPE
Butene Copolymer (Low slip and antiblock)Applications: Thin gauge blown filmThin gauge blown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, cove..
Dart Drop 2.56 g/micron
65.0 g/mil
Cast Film at 1.25 mil; ASTM D-1709
Chevron Phillips MarFlex® 4553 Polyethylene; LDPE
Low density polyethylene. This LDPE is tailored for cast film applications that require: High speed extrusionLow neck-inGood drawdownEdge tear resistanceLow coefficient of friction Applications: ..
Dart Drop 2.56 g/micron
65.0 g/mil
Blown Film at 1.25 mil; ASTM D-1709
Chevron Phillips MarFlex® 4571 Polyethylene; LDPE
Low density polyethylene. This LDPE is tailored for cast film applications that require: High speed extrusionLow neck-inGood drawdownEdge tear resistanceHigh coefficient of friction Applications:..