Polymer Property : Dart Drop = 153 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 6.04 g/micron
153 g/mil
ASTM D1709A
Westlake EMAC® SP2242 Specialty Copolymer  (discontinued **)
EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo..