Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 15.7 g/micron | 400 g/mil | Blown Film at 1 mil; ASTM D-1709 |
Chevron Phillips MarFlex® 7105FL Polyethylene; LLDPE
(discontinued **) Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a.. |
|||
Dart Drop | 15.7 g/micron | 400 g/mil | ASTM D1709 |
Huntsman Rexell® V8801 Cast Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and.. |
|||
Dart Drop | 15.7 g/micron | 400 g/mil | ASTM D1709A |
Westlake Mxsten CV77518 Polyethylene Plastomer Mxsten CV Plastomer CV77518 resin is a polyethylene plastomer designed for blown and cast film extrusion that contains no slip and no antiblock additives. Films produced with this resin exhibit a ve.. |
|||
Dart Drop | 15.7 g/micron | 400 g/mil | ASTM D1709 |
Huntsman Rexell® V8403 Cast Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and.. |