Polymer Property : Dart Drop = 113.3 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 4.461 g/micron
113.3 g/mil
ASTM D1709
ExxonMobil LD 302.20 High Clarity, High Impact Film Resin
LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information ..
Dart Drop 4.461 g/micron
113.3 g/mil
ASTM D1709
ExxonMobil LD 302.32 High Clarity, High Impact Film Resin
LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information ..
Dart Drop 4.461 g/micron
113.3 g/mil
ASTM D1709
ExxonMobil LD 302.34 High Clarity, High Impact Film Resin
LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information ..
Dart Drop 4.461 g/micron
113.3 g/mil
ASTM D1709
ExxonMobil LD 302.56 High Clarity, High Impact Film Resin
LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information ..
Dart Drop 4.461 g/micron
113.3 g/mil
ASTM D1709
ExxonMobil LD 306.38 High Clarity, High Impact Film Resin
LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical
Dart Drop 4.461 g/micron
113.3 g/mil
ASTM D1709
ExxonMobil LD 306.57 High Clarity, High Impact Film Resin
LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical
Dart Drop 4.461 g/micron
113.3 g/mil
ASTM D1709
ExxonMobil LD 306.75 High Clarity, High Impact Film Resin
LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical