Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM D1922 |
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 0.5 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es.. |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM D1922 |
ExxonMobil Escorene® LD-133 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo.. |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM D1922 |
ExxonMobil EXACT™ 4053 Cast Plastomer Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with poly.. |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM D1922 |
ExxonMobil LD 307.76 Clear, High Impact Film Resin LD 307.76 film has superior impact strength and heat sealability, used in frozen and other food packaging, and high strength bags.Information provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM D1922 |
ExxonMobil LD 312.09 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM D1922 |
ExxonMobil LD 312.23 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM D1922 |
ExxonMobil LD 312.82 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM D1922 |
ExxonMobil LD 334.57 Clear, High Impact Film Resin LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM D1922 |
ExxonMobil LD 334.82 Clear, High Impact Film Resin LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM D1922 |
ExxonMobil LDPE LD 312.23 Low Density Polyethylene Resin Product Description: LD 312 resins are 4.6% vinyl acetate copolymers for films with good toughness. The comonomer content and low melt index of those resins help produce films which exhibit superior.. |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM D1922 |
ExxonMobil LDPE LD 312.82 Low Density Polyethylene Resin Product Description: LD 312 resins are 4.6% vinyl acetate copolymers for films with good toughness. The comonomer content and low melt index of those resins help produce films which exhibit superior.. |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM D1922 |
ExxonMobil LDPE LD 362BR Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM D1922 |
ExxonMobil LDPE LD 362BW Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM D1922 |
ExxonMobil LDPE LD 362HE Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM D1922 |
ExxonMobil LDPE LD 362ON Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM D1922 |
ExxonMobil LDPE LD 363BR Low Density Polyethylene Resin Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab.. |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM D1922 |
ExxonMobil LDPE LD 363BW Low Density Polyethylene Resin Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab.. |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | gF; ASTM D1922 |
Braskem F2022/0 Cast Film Extrusion Low Density Polyethylene Films for diapers and absorbent articles; Medium resistance films or for general use.Information provided by Braskem. |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | ASTM-D1922 |
Braskem F2022/0 LDPE Cast Film Extrusion Polyethylene LDPE F2022/0 has excellent sealing characteristics and optical properties with well balanced mechanical properties. Its applications include: general purpose which require no additives; shrink film.. |
|||
Elmendorf Tear Strength TD | 90 g | 90 g | gF; ASTM D1922 |
Braskem BF0323HC Blown Film Extrusion Low Density Polyethylene Heavy-duty bags; Agriculture, Coextruded and shrink films for pallets.Information provided by Braskem. |