ExxonMobil LDPE LD 312.23 Low Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Exxon Chemical
Trade Name LDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LDPE LD 312.23 Low Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LD 312 resins are 4.6% vinyl acetate copolymers for films with good toughness. The comonomer content and low melt index of those resins help produce films which exhibit superior impact strength, good heat sealability and good low temperature properties.Availability: Latin America, North America and South America Additive: Antiblock: 5000 ppmSlip: 1100 ppm Thermal Stabilizer: YesApplications: Coextrusion FilmsFoamsForm Fill and Seal PackagingFreezer FilmLamination FilmPoultry BagProduce BagsRice BagsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ExxonMobil method
Vinyl Acetate Content 4.6 %
4.6 %
ExxonMobil Method
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 5000 ppm
5000 ppm
Slip Level 1100 ppm
1100 ppm
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 170 %
170 %
ASTM D882
Film Elongation at Break, TD 560 %
560 %
ASTM D882
Puncture Energy 0.463 J
0.342 ft-lb
ExxonMobil Method
Elmendorf Tear Strength MD 190 g
190 g
ASTM D1922
Elmendorf Tear Strength TD 90 g
90 g
ASTM D1922
Dart Drop Test 200 g
0.441 lb
ASTM D1709A
Film Tensile Strength at Break, MD 248 MPa
36000 psi
ASTM D882
Film Tensile Strength at Break, TD 23.4 MPa
3400 psi
ASTM D882
1% Secant Modulus, MD 138 MPa
20000 psi
ASTM D882
1% Secant Modulus, TD 165 MPa
24000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 221 °C
<= 430 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 8.5 %
8.5 %
ASTM D1003
Gloss 66 %
66 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 7 lbf
ExxonMobil Method