Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 590 g | 590 g | ASTM D1922 |
M. Holland Company MAGMA® LL1091 LLDPE
(discontinued **) Features: Good Heat Seal, Good ToughnessUses: PackagingProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Elmendorf Tear Strength TD | 590 g | 590 g | ASTM D1922 |
LyondellBasell Plexar® PX3227 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE General DescriptionPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins a.. |
|||
Elmendorf Tear Strength TD | 590 g | 590 g | |
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4202 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance with good optics. It is designed for cast films used in food packaging applications. It com.. |
|||
Elmendorf Tear Strength TD | 590 g | 590 g | |
Dow ATTANE™ 4402 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4402 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance, and outstanding stretchability. It is designed for industrial/consumer cast film applicati.. |
|||
Elmendorf Tear Strength TD | 590 g | 590 g | ASTM-D1922 |
Braskem Pluris 9310 LLDPE Blown Film Extrusion Polyethylene Quatropolymer Pluris 9310 is a Braskem Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conve.. |