Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 518 g | 518 g | ASTM D1922 |
Dow DOWLEX™ 2267G Linear Low Density Polyethylene A high performance stretch film resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |