Polymer Property : Elmendorf Tear Strength TD = 518 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 518 g
518 g
ASTM D1922
Dow DOWLEX™ 2267G Linear Low Density Polyethylene
A high performance stretch film resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow