Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 418 g | 418 g | ASTM D1922 |
LyondellBasell Plexar® PX1164 Extrudable Tie-Layer Resin - Anhydride Modified EVA General DescriptionPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins a.. |