Elmendorf Tear Strength TD 418 g
418 g
ASTM D1922
LyondellBasell Plexar® PX1164 Extrudable Tie-Layer Resin - Anhydride Modified EVA
General DescriptionPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins a..