Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 240 g | 240 g | ISO 6383-2 |
Topas Advanced Polymers TOPAS® 9506F-500 Cyclic Olefin Copolymer (COC) TOPAS® 9506F-500 is a high clarity extrusion grade for use in shrink, food and medical packaging as either a discrete layer in multilayer film or in blends with polyethylene. It is designed to del.. |
|||
Elmendorf Tear Strength TD | 240 g | 240 g | ASTM D1922 |
ExxonMobil LD 117.85 Blown Overwrap Film Resin Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac.. |
|||
Elmendorf Tear Strength TD | 240 g | 240 g | ASTM D1922 |
ExxonMobil LDPE LD 117.85 Low Density Polyethylene Resin Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac.. |
|||
Elmendorf Tear Strength TD | 240 g | 240 g | |
Dow LDPE 609A Low Density Polyethylene, High Clarity Film Grade DOW LDPE 609A resin is a fully formulated high strength clarity film resin for optical packaging applications, such as produce and bakery film. It contains medium levels of slip additive and low lev.. |
|||
Elmendorf Tear Strength TD | 240 g | 240 g | ASTM-D1922 |
Braskem TS7010 LDPE Blown Film Extrusion Polyethylene TS7010 is a low-density polyethylene (LDPE) that presents excellent processability and good mechanical properties. The incorporated additives package warrants a low coefficient of friction (COF) all.. |