Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 66.9 MPa | 9700 psi | ASTM D638 |
Saint-Gobain Meldin® 7021 Direct Formed Graphite Filled Polyimide Finished parts and basic shapes made from 15% by weight graphite filled polyimide material for applications high wear resistance, good thermal oxidative stability, and high temperature resistance. .. |
|||
Tensile Strength, Ultimate | 66.9 - 145 MPa | 9700 - 21000 psi | Average value: 109 MPa Grade Count:17 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |