Tensile Strength, Ultimate 660 MPa
95700 psi
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel
Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr..
Tensile Strength, Ultimate 660 MPa

@Temperature 150 °C
95700 psi

@Temperature 302 °F
EN min.; EN 10002-5
Outokumpu SAF 2507® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Tensile Strength, Ultimate 660 MPa
95700 psi
Haynes 556® alloy, bar after 16000 hours at 537°C
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Ultimate 660 MPa

@Temperature 550 °C
95700 psi

@Temperature 1020 °F
Annealed prior to test
Special Metals NIMONIC® Alloy 75
A nickel-chromium alloy with good mechanical properties and oxidation resistance at high temperatures. Used for sheet-metal fabrications in gas-turbine engines, for components of industrial furnace..