Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 936 MPa | 136000 psi | Hardened 1900°F, Tempered 1200°F |
ATI Allegheny Ludlum 425 Mod Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Ultimate | 936 MPa | 136000 psi | Typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 649°C (1200°F) Temper Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai.. |