Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 572 - 634 MPa | 83000 - 92000 psi | |
Eagle Brass 260 Cartridge Brass, Extra Hard Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Tensile Strength, Ultimate | 552 - 634 MPa | 80000 - 92000 psi | |
Eagle Brass 715 Copper Nickel 30%, Extra Hard 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |