Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 62.16 MPa | 9015 psi | ASTM D412 |
Lubrizol Estane® ALR CL87A Thermoplastic Polyurethane Type: Estane® ALR CL87A is an aliphatic, polycaprolactone-based TPU with a Shore A Durometer of 85-90.Features: Contains a UV package that enhances outdoor weatherability. This high performance re.. |