Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 9.611 MPa | 1394 psi | post cured- 4 hours at 200°C; ASTM D412 |
Multibase SILASTIC® Q7-4850 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tensile Strength, Ultimate | 9.611 MPa | 1394 psi | no post cure; ASTM D412 |
Multibase C6-540 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Ultimate | 9.611 MPa | 1394 psi | EPDM Rubber Hi-K Stress Control Tube; ASTM D42-68 |
3M 4605 Silicone Rubber Termination Kit 3M™ 4604 and 4605 Quick Term II Silicone Rubber Termination Kits are three-piece Cold Shrink terminations for Tape Shield, Wire Shield, and LC Shield power cables. They meet the requirements of IEE.. |
|||
Tensile Strength, Ultimate | 9.611 MPa | 1394 psi | EPDM Rubber Hi-K Stress Control Tube; ASTM D42 |
3M 5360K Silicone Rubber Termination Kits 3M™ 5630K and 5690K Series Quick Term II Silicone Rubber Termination Kits are one-piece Cold Shrink™ terminations for Tape Shield, Wire Shield and UniShield® power cables. They meet the requireme.. |
|||
Tensile Strength, Ultimate | 9.611 MPa | 1394 psi | EPDM Rubber Hi-K Stress Control Tube; ASTM D42-68 |
3M 5600 Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink 5600 and 5680 Series QT-II Termination Kits contain one-piece silicone rubber terminations designed for concentric neutral (CN) cable. They meet the requirements of IEEE 48-1990 for.. |
|||
Tensile Strength, Ultimate | 9.611 MPa | 1394 psi | EPDM Rubber Hi-K Stress Control Tube; ASTM D42 |
3M 5640 Silicone Rubber Termination Kits 3M™ 5640 and 5650 Series Quick Term II Silicone Rubber Termination Kits are one-piece Cold Shrink™ terminations for Jacketed Concentric Neutral (JCN) power cable. They meet the requirements of IEE.. |
|||
Tensile Strength, Ultimate | 9.611 MPa | 1394 psi | EPDM Rubber Hi-K Stress Control Tube; ASTM D42 |
3M 5650 Silicone Rubber Termination Kits 3M™ 5640 and 5650 Series Quick Term II Silicone Rubber Termination Kits are one-piece Cold Shrink™ terminations for Jacketed Concentric Neutral (JCN) power cable. They meet the requirements of IEE.. |
|||
Tensile Strength, Ultimate | 9.611 MPa | 1394 psi | EPDM Rubber Hi-K Stress Control Tube; ASTM D42-68 |
3M 5680 Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink 5600 and 5680 Series QT-II Termination Kits contain one-piece silicone rubber terminations designed for concentric neutral (CN) cable. They meet the requirements of IEEE 48-1990 for.. |
|||
Tensile Strength, Ultimate | 9.611 MPa | 1394 psi | EPDM Rubber Hi-K Stress Control Tube; ASTM D42 |
3M 5690K Silicone Rubber Termination Kits 3M™ 5630K and 5690K Series Quick Term II Silicone Rubber Termination Kits are one-piece Cold Shrink™ terminations for Tape Shield, Wire Shield and UniShield® power cables. They meet the requireme.. |
|||
Tensile Strength, Ultimate | 9.611 MPa | 1394 psi | EPDM Rubber Hi-K Stress Control Tube; ASTM D42-68 |
3M 4604 Silicone Rubber Termination Kit 3M™ 4604 and 4605 Quick Term II Silicone Rubber Termination Kits are three-piece Cold Shrink terminations for Tape Shield, Wire Shield, and LC Shield power cables. They meet the requirements of IEE.. |