Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.611 MPa
1394 psi
post cured- 4 hours at 200°C; ASTM D412
Multibase SILASTIC® Q7-4850 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase
Tensile Strength, Ultimate 9.611 MPa
1394 psi
no post cure; ASTM D412
Multibase C6-540 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 9.611 MPa
1394 psi
EPDM Rubber Hi-K Stress Control Tube; ASTM D42-68
3M 4605 Silicone Rubber Termination Kit
3M™ 4604 and 4605 Quick Term II Silicone Rubber Termination Kits are three-piece Cold Shrink terminations for Tape Shield, Wire Shield, and LC Shield power cables. They meet the requirements of IEE..
Tensile Strength, Ultimate 9.611 MPa
1394 psi
EPDM Rubber Hi-K Stress Control Tube; ASTM D42
3M 5360K Silicone Rubber Termination Kits
3M™ 5630K and 5690K Series Quick Term II Silicone Rubber Termination Kits are one-piece Cold Shrink™ terminations for Tape Shield, Wire Shield and UniShield® power cables. They meet the requireme..
Tensile Strength, Ultimate 9.611 MPa
1394 psi
EPDM Rubber Hi-K Stress Control Tube; ASTM D42-68
3M 5600 Cold Shrink Silicone Rubber Termination Kits QT-III
3M™ Cold Shrink 5600 and 5680 Series QT-II Termination Kits contain one-piece silicone rubber terminations designed for concentric neutral (CN) cable. They meet the requirements of IEEE 48-1990 for..
Tensile Strength, Ultimate 9.611 MPa
1394 psi
EPDM Rubber Hi-K Stress Control Tube; ASTM D42
3M 5640 Silicone Rubber Termination Kits
3M™ 5640 and 5650 Series Quick Term II Silicone Rubber Termination Kits are one-piece Cold Shrink™ terminations for Jacketed Concentric Neutral (JCN) power cable. They meet the requirements of IEE..
Tensile Strength, Ultimate 9.611 MPa
1394 psi
EPDM Rubber Hi-K Stress Control Tube; ASTM D42
3M 5650 Silicone Rubber Termination Kits
3M™ 5640 and 5650 Series Quick Term II Silicone Rubber Termination Kits are one-piece Cold Shrink™ terminations for Jacketed Concentric Neutral (JCN) power cable. They meet the requirements of IEE..
Tensile Strength, Ultimate 9.611 MPa
1394 psi
EPDM Rubber Hi-K Stress Control Tube; ASTM D42-68
3M 5680 Cold Shrink Silicone Rubber Termination Kits QT-III
3M™ Cold Shrink 5600 and 5680 Series QT-II Termination Kits contain one-piece silicone rubber terminations designed for concentric neutral (CN) cable. They meet the requirements of IEEE 48-1990 for..
Tensile Strength, Ultimate 9.611 MPa
1394 psi
EPDM Rubber Hi-K Stress Control Tube; ASTM D42
3M 5690K Silicone Rubber Termination Kits
3M™ 5630K and 5690K Series Quick Term II Silicone Rubber Termination Kits are one-piece Cold Shrink™ terminations for Tape Shield, Wire Shield and UniShield® power cables. They meet the requireme..
Tensile Strength, Ultimate 9.611 MPa
1394 psi
EPDM Rubber Hi-K Stress Control Tube; ASTM D42-68
3M 4604 Silicone Rubber Termination Kit
3M™ 4604 and 4605 Quick Term II Silicone Rubber Termination Kits are three-piece Cold Shrink terminations for Tape Shield, Wire Shield, and LC Shield power cables. They meet the requirements of IEE..