Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 9.31 MPa | 1350 psi | |
Sylvin Technologies 8950-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 9.31 MPa | 1350 psi | |
Sylvin Technologies 9077-80 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 9.31 MPa | 1350 psi | |
Sylvin Technologies 9950-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 9.31 MPa | 1350 psi | |
Dow Corning SILASTIC® Q7-4735 BIOMEDICAL GRADE ETR ELASTOMER, KIT Two-part, platinum-catalyzed (1:1 by weight), enhanced tear-resistant silicone elastomers are heat cured high consistency silicone rubbers designed for use by customers fabricating medical devices.I.. |
|||
Tensile Strength, Ultimate | 9.31 MPa | 1350 psi | ASTM D638 |
Colorite Polymers 5543 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |