Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 9.02 MPa @Treatment Temp. 150 °C, Time 605000 sec |
1310 psi @Treatment Temp. 302 °F, Time 168 hour |
Heat Aging; ASTM D 412/ASTM D 573 |
Zylog Neoplast® 173 FT EB Thermoplastic Vulcanizate Neoplast 173 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |