Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 461 - 603 MPa @Thickness 2.50 mm |
66900 - 87500 psi @Thickness 0.0984 in |
Cold rolled + annealed sheet |
AK Steel 41003 Ferritic Stainless steel AK Steel 41003 is an economical steel that provides excellent weldability, toughness and fabricating characteristics. This alloy is an excellent choice for applications such as tubing and sheet for.. |