Tensile Strength, Ultimate 620 - 870 MPa
89900 - 126000 psi
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; over 9.5 to 25 mm Thickness (UNS C17000)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 620 - 870 MPa
89900 - 126000 psi
Materion Beryllium Copper Alloy 165 Rod and Bar; H (TD04) Temper; over 9.5 to 25.4 mm (UNS C17000)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 620 - 870 MPa
89900 - 126000 psi
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; over 9.5 to 25 mm Thickness (UNS C17200)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 620 - 870 MPa
89900 - 126000 psi
Materion Beryllium Copper Alloy 25 Rod and Bar; H (TD04) Temper; over 9.5 to 25.4 mm (UNS C17200)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 620 - 870 MPa
89900 - 126000 psi
Materion Beryllium Copper Alloy 25 Tube; H (TD04) Temper; over 9.5 to 25.4 mm o.d. (UNS C17200)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 620 - 870 MPa
89900 - 126000 psi
Materion Beryllium Copper Alloy M25 Rod and Bar; H (TD04) Temper; over 9.5 to 25.4 mm (UNS C17300)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 770 - 870 MPa
112000 - 126000 psi
CLAL-MSX NICLAFOR® 1000 TF Quenched/Precipitation Heat Treated, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..