Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 59.8 MPa | 8670 psi | 5 mm/min; parallel to flow; ASTM D638 |
Asahi Kasei Tenac®-C 8554 Acetal Copolymer, High Flow
(discontinued **) Superhigh-flow grade, with properties necessary for VCR reels.Applications: VCR reels.This product is not a part of the standard product line dated 2003. |