Tensile Strength, Ultimate 59.8 MPa
8670 psi
5 mm/min; parallel to flow; ASTM D638
Asahi Kasei Tenac®-C 8554 Acetal Copolymer, High Flow  (discontinued **)
Superhigh-flow grade, with properties necessary for VCR reels.Applications: VCR reels.This product is not a part of the standard product line dated 2003.
Tensile Strength, Ultimate 59.8 MPa
8680 psi
DIN 53455; ASTM D638
Kolon KOPA® KN173MC M/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..