Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 517 - 586 MPa | 75000 - 85000 psi | |
Materion BrushCAST® 20C High Strength Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 517 - 586 MPa | 75000 - 85000 psi | |
Materion BrushCAST® 21C High Strength Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 517 - 586 MPa | 75000 - 85000 psi | |
Materion BrushCAST® 20CT Fine Grain Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 503 - 586 MPa | 73000 - 85000 psi | |
Eagle Brass 706 Copper Nickel 10%, Extra Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Tensile Strength, Ultimate | 517 - 586 MPa | 75000 - 85000 psi | |
Ametek AM 388™ Alloy (UNS C72650) TD02 1/2 Hard Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |