Polymer Property : Tensile Strength, Ultimate = 8301 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 57.23 MPa
8301 psi
Abatron AboCast 8-11/Abocure 8-11 Epoxy  (discontinued **)
2-part solvent-free dielectric epoxy casting compound.Processing: 100/35 ratio (pbw); Gel time, 100 g (3.5 oz.): 93 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adhe..