Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 0.570 MPa | 82.7 psi | ASTM D 638 |
REXtac Rextac® RT 2315 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Ethylene copolymer and FDA compliantFeatures: Balance of heat resistance, flexibility and stiffness, good wetting, and medium open timeApplications: Component.. |
|||
Tensile Strength, Ultimate | 0.570 MPa | 82.7 psi | ASTM D638 |
Covestro Bayfill® EA 6003 Polyurethane Energy-Absorbing Semi-Rigid Foam, Recoverable Grade, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |