Polymer Property : Tensile Strength, Ultimate = 0.570 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.570 MPa
82.7 psi
ASTM D 638
REXtac Rextac® RT 2315 Amorphous Polyalphaolefin (APAO)
Adhesive and Sealant Grade.Description: Ethylene copolymer and FDA compliantFeatures: Balance of heat resistance, flexibility and stiffness, good wetting, and medium open timeApplications: Component..
Tensile Strength, Ultimate 0.570 MPa
82.7 psi
ASTM D638
Covestro Bayfill® EA 6003 Polyurethane Energy-Absorbing Semi-Rigid Foam, Recoverable Grade, MDI-based 2-Component Liquid System
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.