Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 8.24 MPa | 1190 psi | 500 mm/min; ASTM D 412 |
Zylog Neoplast® 173 FT EB Thermoplastic Vulcanizate Neoplast 173 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |