Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 549 MPa @Temperature 204 °C |
79600 psi @Temperature 399 °F |
|
Haynes Multimet® alloy, sand cast, 1171°C heat treatment for 2 hours Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |